IND-1500 - Nanoindentation Tester

上海仪舶实验室自动化 25-01-23 13:11:09

IND-1500 - Nanoindentation Tester

The quantitative mechanical properties of small volumes of materials can be determined with the help of nanoindentation. At present, this technique is an established process to determine the elastic, plastic, and viscoelastic properties of materials like semiconductors, ceramics, soft films, biological materials, multi-phase metals, hard thin films, and plastics from the micro-scale to the nanoscale.

Nanoindentation

A nanoindentation test provides accurate load-displacement curves for testing on both soft and hard surfaces, including rough surfaces like those made by industrial processes such as thermal spray coatings, by quantitative measurement of the mechanical characteristics of small volumes of materials.

The main applications of these instruments are thin films, biological materials, ceramics, multi-phase, metals, etc. But they can also be applied for viscoelastic measurements of polymers, flexure testing of MEMS, and any application that necessitates mechanical measurement on the sub-micron scale.

Hardness, elastic modulus, and yield strength are the main materials properties measured. Based on the sample, storage and loss moduli, fracture toughness, and scratch and wear properties are also measured

.Semilab

Nanoindentation Tester

The IND-1500 instrument incorporates additional features of the IND-1000 and has been designed to convey a controlled load and deformation of the material under test. The mechanical response of the material is quantified by using force and displacement sensors. The range and resolution of the actuator and the force and displacement sensors are extremely small (in the range of mN and μm with nm and nN resolution).

The high precision of the measurement enables recording of events on the micro-scale to the nanoscale. This allows interpreting and explaining macro-scale damage by events on the sub-micron scale, thereby enabling investigation and customization of the basic properties of the sample for specific applications.

IND-1500 — Nanoindentation Tester

Integrated with the additional features of the IND-1000, the IND-1500 makes use of powerful LVDT sensors for force and depth measurements. In this state-of-the-art package, AC amplification provides a μV noise floor. Exclusive circuitry ensures balancing of the signal to leverage the entire range of the analog-to-digital interface.

Features

High-resolution depth profile for Young’s modulus and hardness

Dynamic and static measurement modes

AFM on the same Z-axis (optional)

Additional optical microscope provided on the same Z-axis

Integrated with scratch tester

Software integration with finite element analysis software

The use of LVDT measurement sensors for nanoindentation applications was pioneered by CSIRO in the late 1980s. From that time, with more experience, the technique has been well established, offering low-noise sub-nanometer resolution in a highly robust package.

When compared to competitor instruments that use a capacitance sensor, the IND system is virtuallyresistant to mechanical breakage due to overloading of the indenter shaft. This is because the indenter shaft directly passes through the sensor and can withstand unintentional deflection of several millimeters without any damage.

The force sensor is completely insulated from the load actuator and directly measures the force applied to the indenter, without any signal subtraction from support springs. The depth and force sensors are calibrated individually against international standards. Closed-loop feedback from the force sensor or the depth sensor can be selected. For high-speed data acquisition, users can even choose the open-loop operation mode.

Advantages of IND-1000

Technology developed based on Fischer-Cripps Laboratories’ effective nanoindentation system

Robust design withstands considerable overuse

PZT expansion element with excellent quality, without heat generation

Measured material properties include hardness, fracture toughness, yield strength, elastic modulus, scratch and wear properties (based on the sample), as well as storage and loss moduli

Periodic calibration not needed

Closed-loop force/depth feedback

Highly linear response LVDT and sub-nanometer depth resolution

Traceable calibration

Real-time feedback control over application of depth- or load-independent force and displacement measurement

Reliable performance for several years

Almost resistant to mechanical breakage when compared to competitor devices

Low compliance load frame, mountingsand enclosure

Easily exchangeable indenter tip

Precise positioning of the sample ensured by video microscope and automated X-Y-Z-movement

IND-1500 — Nanoindentation Tester

Optional Features

Lateral force (Scratch Testing Module)

Atomic force microscope

Integrated finite element analysis module

IND-1500 Benefits

Improved vibration discharge

Enhanced voice isolation

IND-1500 — Nanoindentation Tester

[IND-1500 - Nanoindentation Tester]相关推荐
Lincoln Minerals Limited

Lincoln Minerals Limited

Lincoln Minerals Limited is an Australian company with a portfolio of quality iron ore, nickel-co……...

PacBio

PacBio

At PacBio, we’re devoted to empowering you. Pioneering the future through biology takes vis……...

韩国IVIM Technology

IVIM 技术是基于韩国科学技术院 (KAIST) 开发的创新技术 IntraVital Microscopy (IVM) 而成立的。 IntraV……...

今日仪器
  1. Item North America

    Item North America

    Item North America is a premier provider of precision ball screws for use as a drive mechanism in linear slides, multi-axis motion and complex material handling devices. item ball screws feature hi……

    代理品牌 2025-09-04

  2. Streaming Answers: SurPASS™ 3

    Streaming Answers: SurPASS™ 3

    SurPASS™ 3 is capable of measuring the zeta potential over an extensive range of materials and allows the analysis of varied surface properties and their changes. The zeta potential explains ……

    仪器产品 2025-09-04

  3. AHP Materials

    AHP Materials

    AHP Materials is a specialty materials company focused on the manufacturing and selling of high purity specialty metals and compounds. AHP concentrates mainly on Antimony, Cadmium Sulfide, Telluriu……

    代理品牌 2025-09-04

返回顶部小火箭